Skip to main content

RE: [MW:24352] RE: 24334] Failure Analysis

Seems to me that it was tested above the minimum specified yield strength of the base material (over pressured) because there is a lot of deformation visible on the picture, if material/weld failures were present in general you will get a brittle fracture. Radiographic examination makes only sense if the present fracture surface shows any indication which may relate to an improper longitudinal weld.

I would suggest checking base material certificate (also check wall thickness with requirements) and execute some tests on the uninfluenced base material in order to check if values comply with the certificate.

Also check calibration of equipment used during testing, was it giving the correct information?

 

Also important to know is the procedure followed during testing. For example in which steps was the test pressure applied, and was the temperature of the water / material during testing.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Verzonden: maandag 22 februari 2016 08:55
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:24349] RE: 24334] Failure Analysis

 

If possible, you can also take a radiography in the same line of failure (seam or seamless) 

to check for any defects in that pipe material. 

 

C Sridhar.
Technical Adviser - Welding,
for Alsta Pristine Engineering Private Limited,. Bangalore
( SS, AL fabricators & A venture of Advance Eng. Training & Inspection Services). Chennai,

Mobile nos: 0 94449 71097, 0 7406 326326, .

 

 

Please don't print this e-mail unless you really need to. Save the environment.

 


Life is like bicycling. To move on, keep balancing  throughout.. 


 

 


From: 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; Nachiket Vagal <nachi.vagal@gmail.com>
Sent: Monday, 22 February 2016 10:10 AM
Subject: Re: [MW:24345] RE: 24334] Failure Analysis

 

Thanks, Alan. I have asked for more details as it is of a great general interest to all students of failure analysis. I shall make them available on this forum when received.

 

BR,

Shashank C Vagal 

 

 


From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Monday, 22 February 2016 3:08 AM
Subject: [MW:24341] RE: 24334] Failure Analysis

 

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: 21 February 2016 08:51
To: Bathula Raghuram (Mumbai - PIPING) <r.bathula@ticb.com>; Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24334] Failure Analysis

 

Dear all,

Please suggest what could have caused this pipe failure after Hydrotesting..... Consider all general conditions as all details are not known yet

 

BR,

Shashank C Vagal 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/434548542.6153632.1456044675941.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 

This email has been scanned by BullGuard antivirus protection.

For more info visit www.bullguard.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000801d16cf0%2435111d80%249f335880%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1737111366.6375486.1456116044537.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2051398195.6417657.1456127671999.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...