for given current, dia 1.2 will give deposition than dia 1.6mm--THANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITYOn Wed, Feb 17, 2016 at 2:12 PM, Pravin G <htcispravin@gmail.com> wrote:--Dear Expert,
Greetings of the day.
I have a doubt on welding high strength material YP690, jack-up rig.
Currently we are using E111T1-GM H4, 80%Ar - 20%CO2, 1.2mm wire size.
Recently client is insisting on changing to 1.6mm wire size for higher productivity & efficiency.
However in my opinion, using 1.6mm requires usage of higher welding current 350A & above,
And not all welders are able to handle such high ampere & speed, this might cause some defects.
In addition, my concern is high heat input & cooling rate.
I have explained all this details to client, but client don't accept.
Pravin PoornachandranSent from my iPhone
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9DF94DD3-B375-4B0A-B737-8390C1A1B40B%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOmwXGYy30nnMtG5VEOA1%2BChdRDf%2BEg_bbqZRW6_wipYA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Thursday, February 18, 2016
Re: [MW:24315] Wire size 1.6mm
Dear Sir,
Thank you vey much for your explanation.
Is there any document or graph which I can use to explain to client? Maybe it would be helpful for me.
Sent from my iPhone
Pravin Poornachandran
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment