Re: [MW:24330] RE: 24309] PAUT & TOFD Level III

As I understand PAUT & TOFD are NDE UT technics and not NDE methods. Hence NDE Level III in UT is required with training in special technics.

Regards
P. V. Ghanekar

On 17 Feb 2016 09:39, "pgoswami" <pgoswami@quickclic.net> wrote:

Hi Mostafa,

 

These techniques are very specialized techniques. Not all NDE techs are up to speed with both of these techniques. Please see some guidelines from the BINDT on the same.

 

I'm not sure , where you're located, you may check with the local high profile NDE Schools or Companies, who'll have those personnel in their team

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: Tuesday, February 16, 2016 8:25 AM
To: Materials & Welding
Subject: [MW:24309] PAUT & TOFD Level III

 

Dear Sir,

Kindly clarify if  there is level III in PAUT&TOFD or not. our client insists for level III in PAUT&TOFD for PAUT procedure review and level II in PAUT&TOFD to carry out the work. i searched many but i found NO body has this certificates. are these certificates true? and how can i get it?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855091088.3944591.1455629104764.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAI6C/nhitp9NlnqAyYQt%2BycBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3bb02e17DuzaRdDebdh4JGxca8CVe2--EPFjbSAmxyhGg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...