[MW:24361] Flange Buttering

Dear All,

   In my project Slip on flange to Pipe We have 7 mm gap .. Pipe have ovality 

Now my client saying to us to do buttering at flange at machining 

If we do buttering at flange its allowed in the code book 

Please guide me

Best regards
Sankar.k

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/97c5d7b8-713a-4625-afc8-9bcbd722e7a2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...