He has to be qualified again since he has stopped working for a period longer than 6 months

Sent from my BlackBerry 10 smartphone.
From: Mohd Azam
Sent: Κυριακή, 27 Δεκεμβρίου 2015 - 16:32
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:24008] Welder Qualification as per ASME SEC IX

Dear Expert,

"X" welder working with company and left the organization. Again after Two or three year he is joining back same company. All earlier certificate is available with company with proper documentation.

 

Is it possible to renew his earlier certificate with one sample based on RT or visual inspection OR All new qualification is to be done New. Qualification code is ASME SEC IX.

 

Pls provide your valuable input with standard reference.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXSMVhvN0Fje56BbuQb6V3KSYO%3Dz17%2BLtshZO1u3Vt%2Bkhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...