Wednesday, December 23, 2015

[MW:23997] Iron Dilution in 70-30 Cu-Ni W.D. on P-No. 1 Base Metal.

Dear Experts, 

Greetings of the day. 

 I need your expert advise on an issue. In one of our project, 70-30 Cu-Ni W.D. to be done on P-No. 1 base metal. As per client's Data sheet, 3.0 mm. W.D. is specified. Accordingly we have qualified WPS to get the undiluted chemistry on 3 mm. W.D. from interface as per ASME Sec. IX. But in client's project spec. it is specified- "in case a higher deposition thickness and multiple weld layers are required to achieve the minimum specified undiluted deposit metal, the same shall be done only after taking prior approval of client. Minimum thickness of undiluted finished weld overlay from top shall be 2 mm. or as specified in the drawing. Now, my concern is shall we have to certify undiluted chemistry at 1 mm. from fusion surface considering (3 mm. required W.D. as per Data sheet - 2 mm.) or at 3 mm. viz. top surface. 

Please revert at the earliest. 

 Thanks & regards, 



 C. R. GANDHI

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...