Re: [MW:23945] Preheat requirement for EN10225 material

You may find an answer in EN 1011-2, since you are dealing with EN materials

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


vijay ---04/12/2015 06:46:32---Gents, Please advise for the minimum preheat recommended for EN 10225 S355G7+M &

From: vijay <vijayakumarme@gmail.com>
To: materials-welding@googlegroups.com
Date: 04/12/2015 06:46
Subject: [MW:23944] Preheat requirement for EN10225 material
Sent by: materials-welding@googlegroups.com





Gents,

Please advise for the minimum preheat recommended for EN 10225 S355G7+M & S355G8 + M Z35 steel grade materials for weld procedure qualification with SMAW process.

Regards,
Vijay

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAJ3svCD31EGBwyJy5QR%2BUt2iWLUn90k6ktoYXq_XhGN3ASfpMg%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...