Hi all,

Code: ASME VIII

Condition : PQR/PTC completed with combination of 3 welding process

During testing,  impact test specimen taken as per UG84 but 2 welding process not covered due to some reason
(I.e) all 10x10x55 specimen only cover one process out of 3 process.

After impact testing,  all results are accepted.

Now, Is these accepted results applicable only for tested one process or initial 3 process?

pls reply with appropriate justification

Thanks
Venkatesan
g.venkatesan06@gmail.com
+65 84392538

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACoj_XSc7xw8F-RyXStsw5iT0WX5EYvg5DiB6GRBsM8gcbYmCg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...