Re: [MW:24001] IMPACT EXEMPTION FOR DUPLEX FLANGES SA 182 Gr F51

i guess you should use Appendix JJ, 
UHA -51(g)?


On 24 December 2015 at 13:11, VISHNU <vishnus.2184@gmail.com> wrote:
Dear sir,

I have one query regarding to above subject,

One of the definition of governing thk when using fig. UCS-66 - Governing thickness of flat non welded parts, such as bolted flanges, tubesheet and flat head is the flat component thickness divided by 4

But what about Duplex flanges ? UHA is not giving such clause, so what will be governing thickness to be consider for duplex flanges (SA 182 F51) ?

Thanks in advance

Regards

vishnu 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubncZz_x6w5-DC9nmF_hLrzuDzMByuph%3DHvmbaCOaC%2BUcw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...