Re: [MW:23941] Re: Jacket piping

Look into PIP or the company standards for which you are doing the project

On Wed, Dec 2, 2015 at 7:42 AM, PRASANTH RAJAN <prasanthgalfar@gmail.com> wrote:
Any specified standards or is there any where mention that normal weld neck flange cannot be used in jacket piping

On Wednesday 25 November 2015, PRASANTH RAJAN <prasanthgalfar@gmail.com> wrote:
Dear experts    
  Is it possible for welding of jacket outer pipe on the  the inner pipe flange , its there any standard that allow the welding of pipe in forged material


--
WITH REGARDS
 
*PRASANTH RAJAN*
*MECHANICAL SUPERVISOR*
*GALFAR ENGINEERING EMIRATES*
*prasanthgalfar@gmail.com* <prasanthgalfar@gmail.com>
 




--
WITH REGARDS
 
*PRASANTH RAJAN*
*MECHANICAL SUPERVISOR*
*GALFAR ENGINEERING EMIRATES*
*prasanthgalfar@gmail.com* <prasanthgalfar@gmail.com>
 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKCULh5q5NE-CpwbQYqsubEw%3D2eaFAAdb6TxeSJ8Mrv66%2BNHiA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Ohm Guru Namasivaya

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFj9zKMMBXRLHFK1FnQzD7WcF1bd%2BmsQuRAhaNGu4VcBY2bOSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...