[MW:23974] Qualified Base metal thickness range as per ISO 15614-1 :2012.

Dear All,

Need your help,

I have qualified  fillet weld PQR with following ,

Thickness of Pipe:- 1 mm

Thickness of Plate :- 4 mm

I have confusion about base metal qualification thickness,

 Qualification thickness will be 0.7 mm to 8 mm for single layer for both Pipe & Plate

Or 

For Pipe it is 0.7 to 2 mm &  for plate it is 3-8 mm.

What is correct? 

Thank you

Vijay Katkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrK48dBPO2Sh2jgLyiPWxY2_NUHxRYdYvk7FJhukB53gdA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...