[MW:24014] Re: S.A. 2.5 surface profile

Hello,
No. Without Sand/Grit blast it is not possible to achieve Sa 2.5 cleanliness grade. This grade is only obtained by blasting with various abrasives.

Thanks,
Kiran

On Tuesday, August 18, 2015 at 10:04:06 AM UTC+3, Jasim Ahmed wrote:
Dear experts,

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fc28d76d-199d-4111-b1a9-0b4ed6704b6f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...