Re: [MW:23963] Tensile specimen size

Size will be 50×250 mm

Sent from Yahoo Mail on Android


From:"sajid ahmad" <sajid.qaqc@gmail.com>
Date:Wed, 9 Dec, 2015 at 6:41
Subject:[MW:23961] Tensile specimen size

Dear experts
I have raw material which details are given bellow.
 Material :                SA 516 Grade 70 N
Thickness of Plate: 50 mm
 I observed during inspection that there is missing of plate mark No.So we are conducting Tensile test in order to co-relate with ASME Sec II.
what will be the specimen size?

Regards

M.S.Ahmad 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKkJLfgTkvdo37zehERpkPi_kSQeffMmaYgHGS%2BwB91UeZ2gw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1449635583.17835.YahooMailAndroidMobile%40web192706.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...