Re: [MW:19966] welding rod for ss 301 and ss321

Hi
 
If you are using TIG process then use the following welding consumables:
ER 308 / ER 308L for SS 301
ER 347 for SS 321
 
Regards
 
Prem Nautiyal
Cell: 9769316004


On Thursday, January 30, 2014 5:06 PM, Touqueer Zaman <zaman@desipower.com> wrote:
 We have to weld combustion cone of woody biomass gassifier  of Ankur gassifier system. The metals are ss 301 and ss 321. I would like to know the best electrode to weld these meteal.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...