[MW:19914] ACCEPTANCE OF NACT PLATE INSTEAD OF ONLY NORMALISED

One query related to acceptance of NACT plates instead of only Normalised.

For Shell:
SA 516 GRADE 70 - SOUR - NACE  - SEC VIII-II
THICKNESS - ABOVE 100 MM
PWHT TEMP = 621° C - MIN AS PER NACE
SIMULATION - NORMALISING + 3 PWHT CYCLE


For Heads:
SA 516 GRADE 70 - SOUR - NACE -SEC VIII-II
THICKNESS - ABOVE 100 MM
PWHT TEMP = 621° C - MIN AS PER NACE
SIMULATION - NORMALISING+NORMALISING + 3 PWHT

Que:
 
1. IF HEAT TREATMENT IS CARRIED OUT IS NACT INSTEAD OF NORMALISING THEN MILL IS GIVING THE GUARANTEE FOR ABOVE SIMULATION.

2. ............CAN WE REDUCE THE PWHT TEMPERATURE (LESS THAN 621° C) UP TO WHAT LEVEL ???, ............As some of the Mills are giving guarantee of 4 PWHT cycle with 600°C

Regds/Jignesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...