Friday, January 31, 2014

[MW:19973] clarification in flange inspection

Dear sirs,

1.At one purchase order I found FLANGE 6 IN,CLASS BIA,THICKNESS-M#B-16.5 ,MATERIAL A105,300,RF /125 AARH,WN.

RF/125 AARH  Means what?

2.PIPE 10 IN,CLASS-B1A,THICK-STD B-36.1,MATERIAL-ASTM A106 GR B,BE SEAMLESS,CORBON STEEL,
I Am not having the above standard can any one tell what is the thickness of the pipe and which page it has given in standard.

Thanking you,
S.M.Kabeer ahamed
QUEST-KALKATA

No comments:

[MW:35668] Selection of Filler/Electrode.