[MW:19902] Re: High tensile Stainless steel plate

Dear  Vineet kumar.



SA320 CLass L43..  Find the snapshot.

On Tuesday, 21 January 2014 17:17:35 UTC+5:30, Vineet Kumar wrote:
Dear All,

Please suggest Stainless steel  Plate in ASME Material Specification having following properties:
1) Tensile Strength - 830 Mpa (Min)
2) Yield strength - 620 Mpa ( Min)
3) Elongation - 12 %
4) Hardness - 280 HB

Regards,
Vineet Kumar


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...