Wednesday, January 29, 2014

[MW:19949] How sample do we required for Do Galvanized Material to test

Dear All.
I have to test the Galavanized material as per IS code , My
material description is given below,

Round bars - Dia 40 mm -- 250 nos.
Flat - 50x6mm ---120 nos ,
Flat - 200 x 10 - 2 nos.

So please inform me how many sample should i take to test the
Uniformity of coating , Mass of Zinc Coating , and others

Regards
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...