[MW:19902] Welding consumable for cladded plate SA516 Gr70 with SS316

Dear Expert ,

We have vessel shell plate A516-Gr 70 cladded with SS316 L, For the plate thickness: 25MM-40MM cladded 3mm.

Could you please advise the filler material selection and welding sequence for LS and CS.

I intend to use welding process FCAW and SAW. Or SMAW and SAW.

 