Please note that in ASME Sec. II C for 8018G the elements required the minimum values as mentioned in note G. So the properties of each batch of consumables are not guaranteed to meet the requirement. Please check the test certificates for 8018-G. It is better to select the consumables from8018 B series or C series (specially for Low temp. applications) as per your base material requirement.

(G) In order to meet the alloy requirements of the "G" group, the undiluted weld metal shall have the minimum of at least one of the elements listed in this table. Additional chemical requirements

may be agreed to between supplier and purchaser.






On Tue, Dec 20, 2011 at 10:57 AM, Vivek Pandey <vivek.pande06@gmail.com> wrote:
DEAR EXPERTS

AT this time Iam facing a critcal problem in impact test at minus 47
deg. I have a already existing qualified PQR WITH E 8018G & IMPACT
Tested at -47deg. I have used the same PQR in  vessel production test
at -47deg but this PTC has failed in imapct test of WELD & HAZ at
-47deg we are getting erratic value 10, 12, 90 in weld & 60, 10, 50 in
HAZ

Kindly suggest your opanion  about this problem as soon as possible

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Best Regards,

Nilesh Pathare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...