yes you can use ER70S , You can also use ER8018S2
Sandeep Karnwal
Assistant Professor
(HOD ME Deptt.)
DBGI Saharanpur
+918192000737
On Mon, Dec 23, 2013 at 1:23 PM, waqas suleman <waqas.suleman@gmail.com> wrote:
--
Dear All Members,
I am working on a Saudi Aramco Project, i have to weld 6CS9P Line to 9CC9P (CC= Low Carbon Steel).
I am going to use GTAW Process for it.
My question is can we use E 70S filler wire for this kind of welding between CS to Low Carbon Steel.
Please advice.
Regards,
Waqas Suleman
Project Engineer
Mobile # 00966 59 359 0798
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments