RE: [MW:19700] RE:

Dear Santhosh,

 

Could you explain the situation, if PWHT completed means, the manhole flange is welded with the neck.

 

At this stage why you need machining.

 

If so, how you are going to machine the surface.

 

With regards,

S. Sivasubramanian.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Santosh Dantuluri
Sent: Monday, December 23, 2013 12:14 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:19699] RE:

 

Dear Mr.Bala

Thanks for your quick reply
Can you please explain why we cant perform machining after PWHT and where it was highlighted in the code???

D.Santosh


Date: Mon, 23 Dec 2013 14:26:46 +0530
Subject: Re: [MW:19698] RE:
From: balamuruganqaqc@gmail.com
To: materials-welding@googlegroups.com

No it was not accepted.

 

Thanks,

Bala

 

On Mon, Dec 23, 2013 at 2:20 PM, Santosh Dantuluri <santosh-85@hotmail.com> wrote:


From: santosh-85@hotmail.com

To: welding@googlegroups.com
Subject:
Date: Mon, 23 Dec 2013 14:18:44 +0530



Dear experts,

As per API 650(Storage tank) can we proceed for machining on man hole flange face after stress relieving?

Thanks in advance.

Regards
Santossh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No virus found in this message.
Checked by AVG - www.avg.com
Version: 2014.0.4259 / Virus Database: 3658/6941 - Release Date: 12/22/13

No virus found in this message.
Checked by AVG - www.avg.com
Version: 2014.0.4259 / Virus Database: 3658/6942 - Release Date: 12/22/13

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...