Re: [MW:19649] Impact Requirement as per API 650

Dear Mr Prabakar,
Material 516 Gr 70 Location Dasisland, and Naphtha service
 

 
Thanks & Regards,
 
Mohamed Ali Samsudeen


On Wednesday, 18 December 2013 8:12 AM, Prabhakar Seenivasan <prabhakars84@gmail.com> wrote:
Dear Mohamed Ali,

Can you give some more information about your tnk like Material grade, location of the project area & service etc

Regards
Prabhakar. S



On Mon, Dec 16, 2013 at 8:31 PM, Mohamed ali <mdali2000@yahoo.com> wrote:

Daer All,

I am preparing Material request for Plates Tanks,  Design Temp is 90 deg, Operating temp is 10 deg to 30 deg, thichness of plate is Max 32 mm.

what is the IMPACT requirement as per API 650,
 
Thanks & Regards,
 
Mohamed Ali Samsudeen

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...