As per API 650 there is no PWHT requirement for the shell joints. Only for the nozzles and manholes for the particular material groups and there is a thickness limitation for the excemptional cases. Flush type clean out doors for any material shall be stress relieved.



On 20 December 2013 13:32, Krisanu Bhunia <krisanu.bunty@gmail.com> wrote:

Dear Members,

 

We have crude and petroleum tanks in which shell plates thickness vary from 8 mm to 45 mm and the tanks are constructed by our contarctors. We just want to be sure whether PWHT has to be carried out or not in vertical and horizontal joints. Our contrcator says as per API 650 there will be no PWHT of shell plates. I also refered API 650 but couldnt find any thing about pwht of shell plates. please anyone help me out on this issues, in case pwht is to be carried out for shell plates, kindly provide the reference clause no from API 650.


5.7.4 Thermal Stress Relief. I know but If i am not wrong the below clause is for the flush type cleanout fittings rather than the shell butt welded plates.


Regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...