Friday, December 20, 2013

Re: [MW:19657] difficult position welding

It could be done using Pulsed TIG welding process using a pencil torch, with 25 mm head. This type torches
are available in the commercial market.

 
Sridhar


From: Shipo shipo <shipo.ptj@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 20 December 2013 2:40 AM
Subject: [MW:19655] difficult position welding

what is the best method to welding of piping coil as attached ,it's very small space specially i work in P11 AND P91 materials 

--
     
     BEST REGARDS

    SHAABAN MOHAMED ALI SOLIMAN
      QA/QC DEPARTMENT
     PETROJET MARINE DEPARTMENT
     Mobile: +2 012 27 02 44 53
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...