Re: Re: [MW:18249] As per section IX ( Or Any STD ) What is the maximum thickness limit can be applied for a single pass.


You have not mentioned the thickness of base metal. base metal thickness determines the
maximum weld thickness of single pass.


On Mon, 22 Jul 2013 14:15:04 +0530 wrote
>Dear PKM,
 
Please refer SEC-XI   QW-403.9, 13mm (t Pass > 1⁄2 in. (13 mm)) WELD DEPOSITION IS PERMITED
BUT IN CASE OF MORE THEN 13 MM in a single pass, an increase in base metal thickness beyond
1.1 times that of the qualification test coupon.

 

Regards

Lalit Vadadoriya
Sr.Engineer (Inspection)
Engineers India Limited
Dahej Petrochemical Complex,
Dahej (Gujarat)

 

On Sun, Jul 21, 2013 at 9:11 PM, PK M wrote:


Dear experts,  


 As per section IX ( Or Any STD ) What is the maximum thickness limit can be applied for a
single pass. 




Thanks. 


Pkm.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

 
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

 
 


--




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
---
>
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.
>
For more options, visit https://groups.google.com/groups/opt_out.
>

>

>


Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. +918511180665

Get your own FREE website and domain with business email solutions, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...