RE: [MW:18220] out of straightness

generally Straightness tolerance is 1m / 1mm, not more then 12mm

Thanks & Best Regards,

 

MVSAMY



> Date: Tue, 16 Jul 2013 17:02:56 +0530
> Subject: Re: [MW:18205] out of straightness
> From: jaffarqc1987@gmail.com
> To: materials-welding@googlegroups.com
>
> dear javeed,
> For that tolerence is 100-200mm for 1.5mm above 1000mm is max 4mm
> tolerence.. as per the project requirement we are used in process
> piping
>
> Riyas.m
> QA/QC inspector
>
> On 7/1/13, Jawed Anwar <jawed81@gmail.com> wrote:
> > ** dear all
> > our construction code is B31.3, during line checking for the test
> > pack i found that line is not straight (out of straightnees) upto 4-5 mt
> > ,after that line is deviated from it origin and continue, i am looking for
> > acceptance criteria for it but i did not find it in code and project
> > procedure for fabrication
> > so kindly any one can explain me about this issue./where it is mention
> >
> > *Thanks & best regards*.
> > *Mohammad Jawed Anwar** .*
> > *(welding inspector)*
> > *Mob no # +966569799776.*
> >
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> > http://materials-welding.blogspot.com/
> > http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> >
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
> > ---
> > You received this message because you are subscribed to the Google Groups
> > "Materials & Welding" group.
> > To unsubscribe from this group and stop receiving emails from it, send an
> > email to materials-welding+unsubscribe@googlegroups.com.
> > For more options, visit https://groups.google.com/groups/opt_out.
> >
> >
> >
>
>
> --
> [image: cid:image001.gif@01CE556F.A9109490]
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...