Monday, July 22, 2013

Re: [MW:18246] I need a clarification, is FCAW process comes under gas metal arc welding process?

YES.

QW-492 gives the definition:

welding, flux-cored arc (FCAW):  a gas metal-arc welding
process that uses an arc between a continuous filler metal
electrode and the weld pool. The process is used with
shielding gas from a flux contained within the tubular
electrode, with or without additional shielding from an
externally supplied gas, and without the application of pressure.

Regards

Prem Nautiyal
9769316004



From: Tarek Yehia <t.yehia2009@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, July 22, 2013 10:09 AM
Subject: Re: [MW:18236] I need a clarification, is FCAW process comes under gas metal arc welding process?

Dear Raghuram Bathula,

what is in QW-492?!!


On Mon, Jul 22, 2013 at 7:23 AM, Ravikumar, Thattekere Siddappa <travikumar@flowserve.com> wrote:
Yes it is under gas metal arc welding , which will with flux wel be coated for continuous shielding , weld parameters are slightly variable to GMAW  and the gas consumption will be less compared to GMAW
Regards
TSRK
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula
Sent: 22 July 2013 09:49
To: materials-welding@googlegroups.com
Subject: Re: [MW:18232] I need a clarification, is FCAW process comes under gas metal arc welding process?
 
Yes, refer QW 492
On 21 July 2013 21:12, PK M <pkmqaqc@gmail.com> wrote:
Dear Experts,
I need a clarification, is FCAW process comes under gas metal arc welding process?
 
Thank you.
 
Pkm..
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Best regards,
 
Tarek Yehia

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...