[MW:18292] High Ferrite No.

Dear Experts

Recently I came across an issue of High Ferrite no. in the weld metal.

Parent Metal : A 304L
Weld Metal : 308L
Welding Process : GTAW

The affected area is only a quarter portion (3'o clock to 6'o clock position) of the 30" pipe where ferrite no has been observed as over 21 FN. and PMI has shown 1.57% of Mo. 

Please give your valuable comments and rectification measures for this. Refer the attached photos for clarity.

Thanks and Regards
Harikrishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...