On Sat, Jul 27, 2013 at 5:25 AM, pgoswami <pgoswami@quickclic.net> wrote:
Hi Punit,
 
Please look at this generic  oil and gas standard, page 109-115(both for cold and induction bends). The other good document to follow is ASME B-16.49, standards for induction bends. The presentation of Barry  Crouch gives  a good snapshot of the process and effects of different variables. The soak temperature for duplex and CRA clad pipes could be close, between 1050-1100 Deg C based on piping wall thickness.
 
Prior to performing production, "Qualification Bends" are must to standardize bending parameters, and check the various required mechanical properties  of the bends.  Norsok document (M-630) provides many of such details.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Punit Dubey
Sent: Friday, July 26, 2013 5:20 AM
To: materials-welding@googlegroups.com
Subject: [MW:18266] Induction Bending

Dear Experts

Requesting to share your experience regarding the manufacturing of hot induction bends of INCONEL 825 pipes, Duplex Stainless Steel (ASTM A 815, UNS S31803) pipes and Cladded pipe (CS+ 3 mm Thick CRA - Incoloy 825).
Information required in the terms of bending temperature, cooling method, requirements of post bend heat treatment.  

regards

Punit Dubey

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Best Regards,
Suresh Babu,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...