[MW:18239] Re: I need a clarification, is FCAW process comes under gas metal arc welding process?

Dear Pkm,

Generally, the FCAW process is considered different from that of the GMAW process. The FCAW has the electrode with flux powder filled in the tubular filler, whereas the GMAW has just the filler acting as the electrode. The FCAW is applied quite similar to GMAW, and also sometimes applied along with gas shielding. But the shielding gas is not mandatory requirement, as the case is in GMAW. 

With all due regards,

Dileep Sankar



On Sunday, July 21, 2013 9:12:49 PM UTC+5:30, PK wrote:
Dear Experts,

I need a clarification, is FCAW process comes under gas metal arc welding process?

Thank you.

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...