[MW:18268] API 2b straightness interpretation

Dear All,
 
As per the below clause of API 2B

6.4 STRAIGHTNESS

The maximum allowable straightness deviation in any 10-

ft length shall be

1/8 in. For lengths over 10 ft, the maximum

deviation of the entire length may be computed by the following

formula, not to exceed

3/8 in. in any 40-ft length.

My question is , if we have 40 ft length then we have to consider both the point i.e is any 10 ft it shall be max. 1/8" and total length 3/8" or only the second part.

 

Please advise

 

Regards,

 

Vikas waghmare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...