Re: [MW:18244] As per section IX ( Or Any STD ) What is the maximum thickness limit can be applied for a single pass.

Dear PKM,
 
Please refer SEC-XI   QW-403.9, 13mm (t Pass > 12 in. (13 mm)) WELD DEPOSITION IS PERMITED BUT IN CASE OF MORE THEN 13 MM in a single pass, an increase in base metal thickness beyond 1.1 times that of the qualification test coupon.
 
Regards

Lalit Vadadoriya
Sr.Engineer (Inspection)
Engineers India Limited

Dahej Petrochemical Complex,
Dahej (Gujarat)
 

On Sun, Jul 21, 2013 at 9:11 PM, PK M <pkmqaqc@gmail.com> wrote:
Dear experts,  

 As per section IX ( Or Any STD ) What is the maximum thickness limit can be applied for a single pass. 

Thanks. 

Pkm.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...