Dear Sandeep:

Cooling after welding is quite fast and when temp drops below Martensite Finish (Mf), it retards the transformation of austenite to some extent. SR is very similar to tempering and will help transformation of Retained Austenite (RA) and improves dimensional stability and soft spot issues.

Of course this RA comes out in Alloys with more than 0.3% Carbon content but it may happen in low carbon grades too. Read the following article, you will get the idea.

Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Sun, Jun 30, 2013 at 4:35 PM, sandeep monody <smv.monody@gmail.com> wrote:
Dear Ramon Kondori Sir.


Earlier I was believing  the same what you wrote in the reply.

Regarding the 3rd point u mentioned needs more clarification.,because no microstructure changes during pwht as pwht temperature is below the lower critical temperature of the metal but brittleness/hardness changes.

Please clarify your 3rd point

Sandeep.M.V

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...