Re: [MW:18029] Re: phased array vs. RT

Dear Sir,
 
What is the meaning of Volumetric NDE?
 
Thanks,
 


 
On Tue, Jun 25, 2013 at 9:42 AM, veera raghava kommisetti <kommisetti@gmail.com> wrote:
Volumetric exmaination in-lieu of RT is allowed by code.
PA falls under Volumetric examiantion.
Best option would be PA+ToFD


On Tue, Jun 25, 2013 at 7:31 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
http://www.linkedin.com/groupAnswers?viewQuestionAndAnswers=&discussionID=144891298&gid=122787&commentID=146402448&trk=view_disc&ut=1PWB0HnGhwYRM1

Interesting discussion on the above topic

On Tuesday, December 7, 2010 1:30:16 PM UTC+5:30, Navid Navidi wrote:
Hi all,

is it possible to use phased array technique instead of RT for NDT teast of a pressure vessels.
Does standard allow us to do so?
what is its advantages?

thank you in advance
Saeed

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...