Dear Experts,
 
One of the manufacturer is using XL-CCH electrodes for Hard Facing Weld Overlay on c arbon steel material. (Chromium Carbide Alloy Deposit Hard Facing Electrode).
 
The weld overlay outer surface is showing parallel hair line cracks.
 
The manufacturer is arguing that these cracks are bound to develope due to inherrent properties of electrode & it is good to observe cracks on weld for ensuring the application of these type of electrode. The electrode catalogue also states that cracks can be developed on weld surface.
 
My question is which code/standard allow cracks on such hard facing overlay ?
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...