I have the following doubts, please clarify.
 
1.  A welder is qualified for P-1 with GTAW (11.08mm) & SMAW (14 mm). This welder is also qualified for P5A with GTAW (8mm) & SMAW (Unlimited). Can he weld P1 pipe of thickness 28.58 with GTAW (8 mm) & SMAW (20.58 mm).
 
2. A welder qualified in SS with GTAW cannot weld CS with GTAW as purging gas is not used in CS. Removal of backing is an essential variable for welder qualification. Please correct me If my interpretation is wrong.
 
 
Sumod
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...