If it is 185 (more than specified) and is crack free, it is acceptable. If it is less than 180 (175 degrees in this case), bend it more or ask for a fresh sample...

Swamy

On Monday, June 24, 2013 1:35:33 AM UTC+5:30, Aamir Hussain wrote:
Dear All, 
 
One specimen which need to bend 180 degree but it is bended 175 or 185 degree is it will acceptable for test? What will be the appropriate action?
 
Best Regards,
Aamir Hussain

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...