Dear,

please refer AWS D1.1 clause 5.3.3.3


On Thu, May 30, 2013 at 8:40 AM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
Is it Fused flux or agglomerated  flux. Generally 1:3 (Used flux:: virgin Flux). Use flux recovery system, consult flux manufacturer
Pandithan
Welding consultant


On Thu, May 30, 2013 at 9:30 AM, muthu barathi <muthu_barathi@rediffmail.com> wrote:
You can not reuse the electrode as it might be consumed . For better performance same flux
could be used for twice as it is after reheating then depend upon the condition of flux 60 /40
or 70/30 new / used you can use. used flux must be cleaned.

On Thu, 30 May 2013 09:02:04 +0530 wrote

>Dear Memebers,
We are using SAW process for Carbon Steel welding but i have doubt in reuse of flux .  My
doubt is that on what basis we can reuse the electrode i am not able to find any standard or
guide line for reusing.  We are reusing the fluxes mixed with 20% used and 80% new flux, is it
OK and please give me some information for reusing of flux or mixing of used flux  with new
flux.

Thanks in advance.
Manoj




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
---
>
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.
>
For more options, visit https://groups.google.com/groups/opt_out.
>

>

>


Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. +918511180665

Get your own FREE website and domain with business email solutions, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Best regards,
 
Tarek Yehia

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...