Thursday, May 23, 2013

Re: [MW:17754] Impact test- minimum thk requirement

Thanks Gents.
It is very clear that impact test shall be performed up to 2.5mm thk.
 
Appreciate all your valuable guidance.
 
Best Regards,
Victor.

On Thu, May 23, 2013 at 6:51 AM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
2/3 of 27 joules is also acceptable in some codes
Pandithan
welding consultant

On 5/22/13, Ramin Kondori <raminkondori@gmail.com> wrote:
> *Dear Victor:*
>
> In our project we have similar requirements for Duplex and Super Duplex as
> James mentioned (regardless of thickness) where it requires impact test at
> -46 degC and results should demonstrate average of minimum 27J and no
> result less than 20J).
>
> Regards
> *Ramin Kondori*
> *Sr. QA/QC Engineer
> *
> *SINOPEC*
>
> r.kondori@petroyada.com
> +98-2123592322
> +98-9132150320
>
>
> On Wed, May 22, 2013 at 3:24 PM, james gerald <gerry_tup@yahoo.com> wrote:
>
>> Impact test not required/cannot be performed if the thickness is below
>> 2.5mm.
>>
>> Check with Metallurgy Lab whether they can machine your sample with
>> thickness 3.73mm and perform Impact.
>>
>> If yes, then Impact test need to be performed at -46/-50degC for Duplex.
>>
>> Thanks & Regards
>>
>> J.Gerald Jayakumar
>> 00968-99438165
>>    *From:* victor george <dvgeorge@gmail.com>
>> *To:* materials-welding@googlegroups.com
>> *Cc:* Arul prakash <r.arulprakash@gmail.com>
>> *Sent:* Wednesday, May 22, 2013 2:33 PM
>> *Subject:* [MW:17738] Impact test- minimum thk requirement
>>
>> Hi Experts,
>>
>> Please explain what is the minimum thickness requirement of impact test.
>>
>> Material: A790 S31803 pipe
>> Size: 1/2' Sch 80 (WT- 3.73mm)
>> Sour service
>>
>>
>> Question: Is it possible to do impact test on 3.73 thk?
>>
>>
>> Best Regards,
>> DV.George
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>>
>>
>>   --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...