Dear Mr Pandithan,

First you have to understand the concept of making WPS / PQR.
First step, make PWPS - Proposed welding specification according to your Base metal and
suitable consumables and along with the client requirement / design requirement of product.

Second step, now conduct the procedure test as per proposed welding specification .

Record all details and after completion of test carryout mechanical testing as per base metal
codes then check the test passed as per code requirement / client contract requirement. If the
test passed prepare the PQR . From that PQR now you may prepare WPS and mention the PQR number
at Supporting PQR of the WPS number.

From one PQR you may prepare lot of WPS within acceptable variable essential / non essential
supplementary essential variables.


On Thu, 23 May 2013 11:47:43 +0530 wrote
> Is it required to put WPS no. in PQR, if so pl give code ref

Pandithan

Welding Consultant



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm



The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/groups/opt_out.







Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. +918511180665

Get your own FREE website and domain with business email solutions, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...