Re: [MW:17816] Radiographic Film Interpretation Excess Penetration..

Dear Friend 

In cross country pipeline due to pigging operation there are some limits for the internal reinforcement of weld.Mr. Kurup has already pointed out according to  API 1104 in his reply.I also have the experience in cross country pipeline for gas distribution, in there the acceptance limit for excess penetration was 2mm. Correct me if I am wrong.

Thanks & Regards
LALU R.P

On Mon, May 27, 2013 at 7:28 AM, Dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
Dear Expertise,

I have this issue please anyone clarify me,
One QA/QC- Inspector 20 years Experience person  he rejected one 24" pipe line  RT film   because of excessive penetration by measuring the dimension with a ruler and required the joint to be repaired..
This is Acceptable or Not Acceptable.
if Acceptable where is mentioned the code?
Please clarify me, Because my management take this issue very serious  

Best Regards 
Dominic V.K.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...