Dear Sir
Refer to ASME B16.9 Fig. 1 Maximum Envelope for Welding End Transitions.
NOTES:
(2) The maximum thickness at the end of the component is:
(a) the greater of [tmin + 4 mm (0.16 in.)] or 1.15tmin when ordered on a minimum wall basis
(b) the greater of [tmin + 4 mm (0.16 in.)] or 1.10tnom when ordered on a nominal wall basis
NOTES:
(2) The maximum thickness at the end of the component is:
(a) the greater of [tmin + 4 mm (0.16 in.)] or 1.15tmin when ordered on a minimum wall basis
(b) the greater of [tmin + 4 mm (0.16 in.)] or 1.10tnom when ordered on a nominal wall basis
Best Regards
2013년 5월 23일 목요일 오후 11시 50분 42초 UTC+9, prem nautiyal 님의 말:
--Dear friendsVendor has manufactured seamless pipe fittings SA 234 Gr.WPB like elbows (3" SCH 40, 90 degree) and reducers (6" X 3" SCH 40).Dimensons have to be checked as per ASME B16.9.The under limit on thickness mentioned is - 12.5%.I would like to know the Over Limit on thickness for pipe fittings as per ASME B16.9.RegardsPrem Nautiyal(Sr. Surve
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments