Saturday, May 25, 2013

Re: [MW:17791] WPS no. on PQR

Attachment may be use full to members

Pandithan
Welding Consultant


On Fri, May 24, 2013 at 8:32 PM, rudolf saldanha <rudolf_jude@yahoo.com> wrote:
Dear Mr. Shrini,
I have not gone to QW-200.1 etc that you have quoted in you reply to the query.
But I can decipher from what you have quoted is .....
it means that the WPS shall refer to the PQR that has been used to prepare the WPS. which means the PQR that has been used while preparing the WPS has to be mentioned.

Let us try to understand and answer the question.

The question here is whether WPS no. is required to be mentioned while preparing the PQR.

In my opinion NO.



From: SRINI <kanna.qc@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 23 May 2013, 21:23

Subject: Re: [MW:17774] WPS no. on PQR

Dear Kanagapandian

It shall be mentioned in PQR.

Please go to caluse QW-200.1 (b) & (e)second paragraph

The WPS shall reference the supporting Procedure Qualification
Record(s) (PQR) described in QW-200.2. The
manufacturer or contractor may include any other information
in the WPS that may be helpful in making a Code.

(e) Availability of the PQR. PQRs used to support WPSs
shall be available, upon request, for review by the
Authorized Inspector (AI). The PQR need not be available
to the welder or welding operator.

PQR- is  only one time
WPS-  we prepare many time with in essential limit in supporting PQR. 


On Thu, May 23, 2013 at 5:22 AM, John Henning <jhenning@deltak.com> wrote:
No, it is not required.    See QW-200.2 (b) – Contents of the PQR.  "The completed PQR shall document all essential and , when required supplementary essential variables of QW-250 through QW-280 for each welding process used during welding of the test coupon.  Non-essential and other variables used during the welding of the test coupon may be recorded at the manufacturers or contractors option.  . . . "  There is no requirement for recording a WPS number.
 
Further, regarding the form provided by Sc IX " Form QW-483, see Nonmandatory Appendix B, has been provided as a guide for the PQR.  . . ."
 
See also the last paragraph of QW-100.1 "The PQR documents what occurred during welding the test coupon and results of testing of the coupon.  As a minimum, the PQR shall document the essential variables and other specific information identified in Article II for each process used during welding the test coupon and the results of the required testing.  In addition when notch toughness testing is required for procedure qualification, the applicable supplementary essential variables for each process shall be recorded."
 
For ASME Section IX it is NOT required.   
 
When stating requirements, one should provide Code reference(s) otherwise indicate it is an "opinion".
 
John A. Henning
Welding & Materials
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of james gerald
Sent: Thursday, May 23, 2013 2:15 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17760] WPS no. on PQR
 
Yes it is required.
 
 
 
Thanks & Regards
J.Gerald Jayakumar
00968-99438165
From: kannayeram gnanapandithan <kgpandithan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, May 23, 2013 8:43 AM
Subject: [MW:17758] WPS no. on PQR

Is it required to put WPS no. in PQR, if so pl give code ref
Pandithan
Welding Consultant

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...