Thursday, May 23, 2013

Re: [MW:17771] WPS no. on PQR

Please refer QW-483 of ASME Sec IX, SUGGESTED FORMAT FOR PROCEDURE QUALIFICATION RECORDS (PQR)
wherein WPS Number is mentioned.
 
In my opinion it is always better to mention WPS No. on the PQR.
 
Regards
 
Prem Nautiyal
 

From: kannayeram gnanapandithan <kgpandithan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, May 23, 2013 10:13 AM
Subject: [MW:17758] WPS no. on PQR

Is it required to put WPS no. in PQR, if so pl give code ref
Pandithan
Welding Consultant

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...