[MW:17772] Bend Angle As per ASME Sec. IX

Dear Experts,

We run PQR for the below material:

CENTRALLOY G4852 Micro of Schmidt+Clemens (Cast Pipe) & sample thickness & Dia. is 113.6mm OD x 10.8 mm.

As per  MTC of Base Metals ( CENTRALLOY G4852 Micro - the Elongation Minimum Required is only 8.0%). This material can not be bend @ 180 degree because of low ductility.

Query as below:

The bend test has to be perform as per ASME SEC IX QW-466.1

Please provide the how to calculate the sample thickness for bend specimen (Pls provide example) & minimum Bend Angle to qualify PQR.
Pls provide the code refrence.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...