Re: [MW:16118] What are the criteria to select Stub in or Stub on for Branch connection in Piping?

Some OEMs see insertion of branch pipe in main pipe as obstruction in flow and prevent from this type of joint orientation. They say it will not ensure proper flow in the branch pipe. Fluid inside pipes is also considered as a factor.   
Stub out connections result in fillet welds while stub in result in butt weld
 
Ammar
On Thu, Nov 29, 2012 at 4:53 PM, Samir Mehta <samirmehta.jnd@gmail.com> wrote:
the branch connection for the header with re-pad should be stub-out. The header that does not have re-pad should be stub-in.

Regards
samir

On Thu, Nov 29, 2012 at 1:47 PM, PK M <pkmqaqc@gmail.com> wrote:
Dear Experts,

What are the criteria to select Stub in or Stub on for Branch connection in Piping?

(Or)

How to choose Stub in or Stub on for Branch connection in Piping?


Thanks,

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Samir Mehta
Engineer - Welding & Projects
JPIOS
Abu Dhabi - UAE

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...