Dear Expert
Please help me out regarding a query.
1. If I will be welding 10thk # 20thk plate test coupon of P-No.1 and P-No.11A than how much base metal as well as weld metal will be qualify.
2.Please also give me the interpretation for QW.202.4 (Dissimiler metal thickness clauses) in simple english, taht will be very helpful to me
Regards
Avinash Pandey
Trainee
Welding Dept.
-- To post to this group, send email to materials-welding@googlegroups.com