Monday, December 31, 2012

Re: [MW:16389] TANK BOTTOM PLATES OVERLAP

Dear Lassaad
 
Vaccum box testing is commonly practiced in Botttom plate overlap joint inspection.
Regards
Mohd. Ilyas
On Sun, Dec 30, 2012 at 11:49 PM, Lassaad <lassaad.mokrani@gmail.com> wrote:
Dear Experts,
Is there any NDT method to check the overlap of bottom plates of an API650 built and used Oil steel tank.?
Many thanks
BR

Sent from my iPad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
Thanking You
With Best Regards
Mohammed Ilyas Mohiuddin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...