dear Mr. Manoj
It is may not be simulation test, it shall be production test coupon
requirement, after welding and SR we have to test the PTC.
regards
gsr
On Thu, Dec 20, 2012 at 4:48 PM, manoj john <manojacgnr@gmail.com> wrote:
> Dear experts,
>
> We are using 50 mm thk SA 516 Gr 70 plate for cabriation of clean out door
> assembly for storage tank. As per API 650 clean out doors shall be heat
> treated (PWHT) after welding. The material we received is in normalized
> condition. My question is whether simulation test is required for this
> plates our TPI says we need to carry out simulation test and What is the
> criteria for simulation test? We are using WPS as per ASME SEC IX with
> stress relieving at 620 degree C.
>
> Thanks in advance.
> Manoj
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-